EVALUASI KESTABILAN LERENG BATUAN MENGGUNAKAN Q-SLOPE, KESETIMBANGAN BATAS DAN PROBABILITAS LONGSOR PADA TAMBANG ANDESIT DESA SIDOMULYO
For an open pit mine, the rock slope stability is one of the major significant challenges at every stage in the operation of an open pit mine. It became a concern from the planning until the mining closure. Mining activities in the research location have entered the mining closure phase and produced the final slope that consists of 4 single slopes with an overall slope height of 65m and an angle of 62° that its stability is not yet known. The actual overall slope has discontinuities which affect the potential for failure. Most of the methods used in geotechnical practice for estimating slope stability are based on the traditional limit equilibrium methods. On the other side, very few empirical techniques exist to assess the slope stability. The empirical method of the Q-Slope is a relatively new methodology for assessing the slope stability in terrains built from rock masses. This method was developed over the last decade by Barton and Bar (2015), with modifications to the original Q-System for application in rock slope stability through the parameter of RQD, Jn, Jr, Ja, O-Factor, Jwice, SRFa, SRFb and SRFc. The stability analysis by Q-Slope method has resulted the slope in stable condition because the value of βQ-Slope > βSlope. The factor of safety limit equilibrium method and probability of failure used the actual geometry and Q-Slope geometry is known in stable condition because it fulfils acceptance criteria with FoS ≥ 1,1 and PoF ≤ 37,5% according to the regulation Ministry of Energy and Mineral Resources Decree 1827/K/30/MEM/2018.Pada tambang terbuka, kestabilan lereng menjadi salah satu tantangan utama pada setiap tahapan dalam operasional pertambangan yang menjadi perhatian mulai dari tahap perencanaan hingga tahap penutupan tambang. Kegiatan pertambangan di lokasi penelitian sudah memasuki tahap penutupan tambang dan menghasilkan lereng akhir yang terdiri dari 4 lereng tunggal dengan tinggi lereng keseluruhan 65m dan sudut 62° dengan kondisi yang belum diketahui nilai tingkat stabilitasnya. Lereng keseluruhan aktual memiliki bidang diskontinu sehingga dapat mempengaruhi potensi adanya longsor. Pada umumnya metode yang diaplikasikan dalam kajian geoteknik untuk mengetahui kestabilan lereng didasarkan pada metode kesetimbangan batas. Di sisi lain, masih kurangnya metode empiris yang diaplikasikan untuk penilaian kestabilan lereng tambang. Metode empiris Q-Slope adalah metode baru yang diaplikasikan untuk penilaian kestabilan lereng pada massa batuan. Metode baru ini dikembangkan oleh Barton dan Bar (2015) yang merupakan modifikasi dari metode Q-System yang diaplikasikan untuk kestabilan lereng melalui parameter RQD, Jn, Jr, Ja, O-Factor, Jwice, SRFa, SRFb dan SRFc. Hasil analisis kestabilan lereng dengan metode Q-Slope diketahui bahwa lereng dalam keadaan stabil karena nilai βQ-Slope > βLereng. Tingkat faktor keamanan (FK) metode kesetimbangan batas dan probabilitas longsor (PL) pada setiap lereng tunggal menggunakan geometri lereng actual dan geometri lereng Q-Slope diketahui dalam keadaan yang stabil karena memenuhi kriteria penerimaan dengan nilai FK ≥ 1,1 dan PL ≤ 37,5% sesuai dengan peraturan pada Keputusan Menteri Energi dan Sumber Daya Mineral nomor 1827 K/30/MEM/2018
POTENSI LONGSOR BERDASARKAN ANALISIS KINEMATIK PADA AREA LOW WALL PT. BUKIT ASAM TBK, SITE TANJUNG ENIM, SUMATERA SELATAN
PT. Bukit Asam Tbk is an open-pit coal mining company in Muara Enim, Soutgh Sumatra. In open-pit mining activities, slope stability analysis is carried out to evaluate the mine in order to create a safe mining process. Several types of slope failure are associated with geological structures. This research was conducted to identify the type of landslides in the low wall area of Pit X PT. Bukit Asam Tbk and determine the slope stability factor based on discontinuity data using the scanline method at 8 observation points that represent the lithology of the low wall area. Methods used in this research is kinematic analysis, slope stability analysis on plane slide types and wedge. Based on the kinematic analysis, it was identified that the Pit X low wall area has the potential for plane and wedge type landslides with a relatively stable slopes.PT. Bukit Asam Tbk merupakan perusahaan tambang batubara terbuka yang berada di Muara Enim Sumatra Selatan. Dalam kegiatan penambangan terbuka, analisis kestabilan lereng dilakukan untuk mengevaluasi tambang agar tercipta proses penambangan yang aman. Beberapa jenis keruntuhan lereng berkaitan dengan struktur geologi tertentu. Penelitian ini dilakukan untuk mengidentifikasi tipe longsoran pada area low wall Pit X PT. Bukit Asam Tbk dan menentukan kestabilan lereng berdasarkan data diskontinuitas menggunakan metode scanline pada 8 titik pengamatan yang mewakili seluruh litologi area low wall. Metode penelitian yang digunakan yaitu analisis kinematik dan analisis kestabilan lereng pada tipe longsoran bidang dan baji. Berdasarkan analisis kinematik, teridentifikasi bahwa area low wall Pit X berpotensi terjadinya tipe longsoran bidang dan baji dengan faktor keamanan tergolong stabil
VALIDITAS HASIL PENGUJIAN KADAR TIMBAL SECARA KOMPLEKSOMETRI TERHADAP MODIFIKASI TEKNIK PREPARASI DALAM PRODUK KONSENTRAT TIMBAL SULFIDA
Lead sulfide (PbS) concentrate is derived from the sulfide mineral galena. In nature, galena must first undergo a concentration process to become PbS concentrate. The determination of lead (Pb) content in the PbS concentrate is carried out using complexometric methods, referring to the modified ISO 13545:2000 standard during the preparation stage. In this research, the validity of the test results was assessed using several parameters, including precision test (repeatability and reproducibility), accuracy (%recovery) and estimation of measurement uncertainty. Certified reference material (CRM) Pb353, with a Pb content range of 58.20-64.33% was used as a sample in this study. The results showed an average Pb content of 61.11% for analyst A and 61.00% for analyst B in CRM Pb353. The research successfully met the precision testing requirements for repeatability (RSD 0.46% for analyst A and 0.39% for analyst B < 2/3 coefficient variance (CV) Horwitz 1.44%) and reproducibility (F-test 1.34 < F-table 4,28 and P-value 0.37 > significance level 0.05). Accuracy was also demonstrated with %recovery (analyst A 9.06–100.53% and analyst B 99.23–99.98%), as well as the estimation of measurement uncertainty (μrelative 2.27% < 5%). Therefore, the determination of Pb content using complexometric methods with modified preparation techniques in the PbS concentrate ensures the validity of the results.Konsentrat timbal sulfida (PbS) berasal dari mineral sulfida yaitu galena. Untuk mendapatkan konsentrat PbS, galena di alam harus diolah terlebih dahulu melalui proses konsentrasi. Kadar timbal (Pb) dalam konsentrat (PbS) ditetapkan secara kompleksometri mengacu kepada ISO 13545:2000 yang dimodifikasi pada tahapan preparasinya. Pada penelitian ini dilakukan validitas hasil pengujian menggunakan beberapa parameter meliputi uji presisi (ripitabilitas dan reprodusibilitas), akurasi (nilai perolehan kembali/%recovery), dan estimasi ketidakpastian hasil pengukuran. Pada penelitian ini digunakan CRM Pb353 sebagai sampel uji yang memiliki rentang kadar Pb antara 58,20-64,33%. Dari hasil penelitian diperoleh nilai rata-rata kadar Pb dalam CRM Pb353 sebesar 61,11% untuk analis A dan 61,00% untuk analis B. Penelitian ini telah memenuhi uji presisi secara ripitabilitas (SBR 0,46% untuk analis A dan SBR 0,39% untuk analis B < 2/3 coefficient variance (CV) Horwitz 1,44%) dan reprodusibilitas (Fhitung 1,34 < Ftabel 4,28 dan P-value 0,37 > taraf nyata 0,05). Akurasi dengan %recovery (analis A 99,06–100,53% dan analis B 99,23–99,98%), serta estimasi ketidakpastian hasil pengukuran (µrelatif 2,27% < 5%). Hasil uji Pb secara kompleksometri dengan modifikasi teknik preparasi dalam produk konsentrat PbS telah memenuhi semua parameter validitas hasil uji
OPTIMALISASI PELINDIAN BIJIH MANGAN ASAL TIMOR TENGAH UTARA MENGGUNAKAN H2O2 SEBAGAI PEREDUKSI
Optimization of manganese ore leaching process from North Central Timor, Indonesia has been investigated. The final product of the leaching process was MnSO4. Variables that were optimized during the process were volume of H2O2, reaction temperature, and reaction time. The final products were characterized by FTIR, powder-XRD, XRF, and AAS. Experimental data shows that the optimum conditions for the leaching process were 50 mL H2SO4 4 M, 25 mL H2O2 2 M, in which the reaction was done at room temperature for two hours. This optimum condition resulting in 38.2% of Mn extraction with 96.88% purity. Based on powder-XRD, the products were a mixture of crystalline MnSO4.4H2O, MnSO4.5H2O and [NH4]8[Mn8(SO4)12].Penelitian optimalisasi proses pelindian bijih mangan dari Timor Tengah Utara, Indonesia telah dilakukan. Produk akhir proses pelindian berupa MnSO4. Variabel yang dioptimalkan selama proses pelindian adalah volume H2O2, suhu reaksi, dan waktu reaksi. Produk akhir dikarakterisasi dengan FTIR, powder-XRD, XRF dan AAS. Data hasil penelitian menunjukkan bahwa kondisi optimum proses pelindian untuk mendapatkan MnSO4 adalah 50 mL H2SO4 4 M, 25 mL H2O2 2 M, dan reaksi dilakukan pada suhu ruang selama dua jam. Kondisi optimum ini menghasilkan ekstrasi Mn sebesar 38,2% dengan kemurnian 96,88%. Berdasarkan analisis powder-XRD, produk yang dihasilkan adalah campuran kristal MnSO4.4H2O, MnSO4.5H2O and [NH4]8[Mn8(SO4)12]
PEMASTIAN VALIDITAS PENGUJIAN KADAR SENG SECARA KOMPLEKSOMETRI TERHADAP MODIFIKASI TEKNIK PREPARASI DALAM KONSENTRAT SENG SULFIDA
Sphalerite is one of the sulfide ore minerals that serves as the raw material for zinc sulfide concentrate (ZnS). Sphalerite in nature needs to be processed through a concentration process to become a high-value ZnS concentrate. The determination of zinc (Zn) content in the ZnS concentrate is carried out using complexometric methods, referring to the modified ISO 13658:2000 method in the preparation stage. In this research, the validity of the test results was conducted using several parameters, including precision testing (repeatability and reproducibility), accuracy (recovery and test result comparison with CRM value), and measurement of relative uncertainty in Zn content determination in ZnS concentrate using the modified ISO 13658:2000 method, it is conducted by two analysts. Certified reference material (CRM) O354 with a Zn content range of (49,30±2,46)% was used as a sample in this research. Zinc content in CRM O354 by Analyst X obtained 49.30% with RSD=0.37% and range of Recovery=(99.5-100.6)%, while Analyst Y obtained 49.03% with RSD=0.64% and range of Recovery=(98.1-99.9)%. Mean of results of the determination of Analyst X and Analyst Y is 49.13% with an uncertainty expanded by 1.90% so, Zn content is obtained at (49,13±1,90)% and the relative uncertainty is obtained at 3.87%. The minimum criteria for precision testing in terms of repeatability are RSD<2/3 CV Horwitz, and for reproducibility (F-test), Ftest<Ftable, for accuracy testing in terms of Recovery=(98-102)%, inter-analyst comparison, and test result comparison with CRM value (t-test), ttest<ttable as well as the minimum criteria for measurement of relative uncertainty<5%. Therefore, the test results of the modified ISO 13658:2000 method for Zn determination in ZnS concentrate have fulfilled all the validity parameters of the test results.Sfalerit adalah salah satu mineral bijih sulfida yang menjadi bahan baku konsentrat seng sulfida (ZnS). Sfalerit di alam perlu diolah melalui proses konsentrasi agar menjadi konsentrat ZnS yang tinggi nilai jual. Kadar seng (Zn) dalam konsentrat ZnS ditetapkan secara kompleksometri mengacu ISO 13658:2000 yang dimodifikasi pada tahap preparasi. Penelitian ini bertujuan untuk memastikan validitas hasil penetapan kadar Zn dalam Konsentrat ZnS metode modifikasi ISO 13658:2000 relatif yang dilakukan oleh dua orang analis dengan parameter uji kinerja metode meliputi presisi (Ripitabilitas dan reprodusibilitas), akurasi (Persen perolehan kembali dan perbandingan hasil uji terhadap nilai benar dalam sertifikat CRM), dan perhitungan ketidakpastian relatif. Sampel yang digunakan yaitu certified reference material (CRM) O354 matriks konsentrat seng sulfida yang memiliki kadar Zn sebesar (49,30±2,46)%. Hasil penetapan Zn dalam CRM O354 oleh Analis X diperoleh rerata sebesar 49,23% dengan RSD=0,37% dan rentang Recovery=(99,5-100,6)% sedangkan Analis Y diperoleh rerata sebesar 49,03% dengan RSD=0,64% dan rentang Recovery=(98,1-99,9)%. Rerata hasil penetapan Analis X dan Analis Y sebesar 49,13% dengan ketidakpastian gabungan diperluasnya sebesar 1,90% sehingga kadar Zn diperoleh sebesar (49,13±1,90)% maka ketidakpastian relatif (KR) diperoleh sebesar 3,87%. Kriteria minimum evaluasi kinerja metode dengan uji presisi secara ripitabilitas yaitu RSD<2/3CV Horwitz dan reprodusibilitas (Uji F) yaitu Fhitung<Ftabel sedangkan kriteria minimum uji akurasi dengan persen perolehan kembali yaitu Recovery=(98-102)% sedangkan kriteria minimum perbandingan hasil uji terhadap nilai benar dalam sertifikat CRM (Uji t) yaitu thitung<ttabel dan kriteria dari ketidakpastian relatif (KR) yaitu <5%. Hasil evaluasi validitas penetapan Zn dalam Konsentrat ZnS menggunakan metode modifikasi ISO 13658:2000 telah memenuhi semua parameter validitas hasil uji
RANCANGAN GEOMETRI PELEDAKAN YANG EFISIEN UNTUK MENDAPATKAN DISTRIBUSI UKURAN FRAGMENTASI BATU GAMPING
The rock fragmentation distribution resulting from blasting is one of the important factors of the blasting method design model for dismantling excavated materials. Calculation of rock fragmentation resulting from blasting using the RL theory. Ash, CJ. Konya, and ICI-Explosive. The method for determining the size of rock fragmentation resulting from blasting and analysis of the fragmentation size distribution in blasting activities uses the Kuz-Ram method and Split Desktop 4.0 software. A good blasting geometry design from a technical and economical point of view enables achieving target production according to the design made by the company in producing an average fragmentation size of limestone <50 cm. Blasting geometry applied by PT. Semen Padang produces a hole volume of 275 m3 with a fragmentation of 53.46 cm. The results of the fragmentation design are based on the RL Ash theory and the Kuz-Ram method with a volume of300.67 m3each hole anda fragmentation size of 50.07 cm, CJ. Konya analysis resulted in a hole volume of 422.4 m3 with an average fragmentation of 44.17 cm, and ICI-Explosive method resulted in a hole volume of 285 m3 with an average fragmentation of 47.86 cm. Based on blasting geometry calculation, fragmentation analysis and economic calculations, it is shown that the blasting geometry suggestion using CJ Konya theory is more optimal and feasible to apply because it results in a larger hole blasting volume, higher percentage of fragmentation of <50 cm which is compatible with the bucket capacity, as well as higher revenue and profit compared to the other two methods.Distribusi fragmentasi batuan hasil peledakan menjadi salah satu faktor penentu keberhasilan dari model rancangan metode peledakan untuk pembongkaran material galian. Perhitungan fragmentasi batuan hasil peledakan menggunakan teori R.L. Ash, C.J. Konya, dan ICI-Explosive. Metode untuk mengetahui ukuran fragmentasi batuan hasil peledakan dan analisis distribusi ukuran fragmentasi pada kegiatan peledakan menggunakan metode Kuz-Ram dan software Split Desktop 4.0. Desain rancangan geometri peledakan yang baik dari segi teknis dan ekonomis dapat menghasilkan target produksi sesuai dengan rancangan yang dibuat oleh perusahaan dalam menghasilkan ukuran fragmentasi rata-rata batu gamping <50 cm. Geometri peledakan yang diterapkan oleh PT. Semen Padang menghasilkan volume perlubang 275 m3 dengan fragmentasi 53,46 cm. Hasil dari rancangan fragmentasi berdasarkan pada teori R.L. Ash dan metode Kuz-Ram menghasilkan volume perlubang sebesar 300,67 m3 dan ukuran fragmentasi sebesar 50,07 cm. Sementara itu, analisis metode C.J. Konya menghasilkan volume perlubang sebesar 422,4 m3 dengan ukuran fragmentasi rata-rata 44,17 cm, dan metode ICI-Explosive menghasilkan volume perlubang sebesar 285 m3 dengan ukuran fragmentasi rata-rata 47,86 cm. Berdasarkan perhitungan geometri peledakan, analisis fragmentasi serta perhitungan keekonomian menunjukkan bahwa geometri peledakan usulan menggunakan teori C.J. Konya lebih optimal dan memungkinkan untuk diterapkan karena menghasilkan volume peledakan perlubang yang lebih besar, persentase fragmentasi <50 cm yang lebih tinggi sesuai dengan kapasitas bucket, serta total pendapatan dan keuntungan yang lebih besar dibandingkan dengan dua metode lainnya