Durabilité de produits innovants de robinetterie en polyamide 6,6
PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques
Durability of innovative valve products in polyamide 6,6
Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques.PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes
Durabilité de produits innovants de robinetterie en polyamide 6,6
PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques
Durabilité de produits innovants de robinetterie en polyamide 6,6
PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques
Durabilité de produits innovants de robinetterie en polyamide 6,6
PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques
Durabilité de produits innovants de robinetterie en polyamide 6,6
PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques
Durabilité de produits innovants de robinetterie en polyamide 6,6
Le PA 6,6 est maintenant envisagé pour des pièces de robinetterie sur le réseau domestique de distribution d'eau potable. Cependant, ce matériau ne pourra être utilisé que si sa durabilité à long terme, en conditions réelles de service, est clairement démontrée. L'analyse cinétique des principaux mécanismes de vieillissement chimique susceptibles de se produire et d'interagir sur le réseau domestique de distribution d'eau potable : l'hydrolyse, la thermo-oxydation et l'attaque chimique par le dioxyde de chlore, a permis au final d'élaborer un modèle cinétique général de dégradation du PA 6,6. Ce modèle donne accès aux modifications structurales du PA 6,6 aux différentes échelles pertinentes (moléculaire, macromoléculaire, morphologique et macroscopique) en conditions de service. Il prédit la fragilisation du PA 6,6 lorsque la masse molaire moyenne en nombre atteint une valeur critique de l'ordre de 17 kg/mole. De nombreuses perspectives de recherche sont présentées comme l'introduction de ce modèle cinétique dans les codes courants de calcul mécaniques.PA 6,6 is now considered for the elaboration of valve parts in the domestic network of drinking water distribution. However, this material will be used only if its long-term durability, in real use conditions, is clearly demonstrated. The kinetic analysis of the main chemical ageing mechanisms which may occur and interact in the domestic network of drinking water distribution: hydrolysis, thermal oxidation and chemical attack by chlorine dioxide, has allowed to finally build a general kinetic model for PA 6,6 degradation. This model gives access to PA 6,6 structural modifications at the different pertinent scales (molecular, macromolecular, morphological and macroscopic scales) in use conditions. It predicts the embrittlement of PA 6,6 when the number average molar mass reaches a critical value of the order of 17 kg/mole. Many research prospects are presented such as the introduction of this kinetic model in common mechanical calculation codes.PARIS-Arts et Métiers (751132303) / SudocSudocFranceF
Going Beyond Counting First Authors in Author Co-citation Analysis
The present study examines one of the fundamental aspects of author co-citation analysis (ACA) - the way co-citation
counts are defined. Co-citation counting provides the data on which all subsequent statistical analyses and mappings
are based, and we compare ACA results based on two different types of co-citation counting - the traditional type that
only counts the first one among a cited work's authors on the one hand and a non-traditional type that takes into
account the first 5 authors of a cited work on the other hand. Results indicate that the picture produced through this non-traditional author co-citation counting contains more coherent author groups and is therefore considerably clearer. However, this picture represents fewer specialties in the research field being studied than that produced through the traditional first-author co-citation counting when the same number of top-ranked authors is selected and analyzed. Reasons for these effects are discussed
Thermal oxidation kinetics of additive free polyamide 6-6
Thermal aging of an additive free PA 6-6 has been elucidated at 90, 100, 120, 140, 150 and 160 C in airventiled ovens by Fourier transform infrared spectrophotometry, viscosimetry in molten state and uniaxial tensile testing. Oxidation of methylene groups starts after a considerably shorter induction period but reaches a lower maximal rate than in additive free PE. Cleavage of CeN bonds constitutes the main source of chain scissions. It leads to the formation of aldehyde chain-ends and a catastrophic decrease in molar mass. Embrittlement occurs at a very low conversion ratio of the oxidation process, in particular when the concentration of aldehyde chain-ends reaches a critical value of [PH¼O]F z 5.6 10 3 mol l 1, corresponding to a critical value of the number average molar mass ofMnFz17 kg mol 1. At this stage, the entanglement network in the amorphous phase is deeply damaged. A non-empirical kinetic model has been derived from the oxidation mechanistic scheme previously established for PE, but improved by adding elementary reactions specific to polyamides such as the rapid decomposition of unstable hydroxylated amide groups. This model describes satisfyingly the main features of the thermal oxidation kinetics of PA 6-6, but also of other types of aliphatic polyamides studied previously in the literature such as: PA 6, PA 12 and PA 4-6, as long as it is not controlled by oxygen diffusion. At the same time, it confirms the existence of an universal character for the thermal oxidation kinetics of aliphatic polyamides whatever their origin, i.e. their initial molar mass, crystallinity ratio, concentration of impurities, structural irregularities, etc
- …