The Latin American Giant Observatory (LAGO) consists of a network of water Cherenkov detectors (WCDs) installed in the Latin American region at various latitudes, from Sierra Negra in Mexico ,and altitudes from Lima, Peru at 20 m a.s.l. to Chacaltaya, Bolivia at 5500 m a.s.l. to the Antarctic Peninsula. The detectors of the network are built from commercial water tanks, so they have several geometries (cylindrical in general) and different water purification methods. All these features generate different profiles in the response to air shower particles measured by our detectors and produce pulse-shaped electronic signals. Common sources of noise in a WCD come from light leakage, electronic noise, and noise associated with the operation of photomultiplier tubes (PMTs) such as thermionic emission and after-pulses; they all could produce detectable pulses recorded by the LAGO data acquisition (DAQ) system. In LAGO WCDs, these noise signals are expected to present a short pulse width (of a few nanoseconds), while secondary radiation typically produces pulses of several tens of nanoseconds.We used data from the LAGO DAQ system, which digitises pulses at 40 MHz sampling rate on windows of 300 ns (12 temporal bins) and with a 10-bit resolution. The LAGO DAQ configuration uses a single threshold-based trigger in the third temporal bin. We proposed a secondary trigger threshold at the fourth bin to improve the noise rejection. In this work, we show how the optimal values for these triggers are now obtained from the measurement of the muon lifetime within the water volume and the resulting Michel spectrum. Our results were also simulated using the LAGO ARTI simulation framework to estimate the expected flux of secondary particles at the detector site; and the Meiga framework, a Geant4-based simulator used to estimate the WCDs response to the atmospheric radiation flux.Fil: Otiniano, L.. Universidad Nacional de Ingenieria; PerúFil: Taboada Nuñez, Alvaro. Consejo Nacional de Investigaciones Científicas y Técnicas. Oficina de Coordinación Administrativa Parque Centenario. Instituto de Tecnología en Detección y Astropartículas. Comisión Nacional de Energía Atómica. Instituto de Tecnología en Detección y Astropartículas. Universidad Nacional de San Martín. Instituto de Tecnología en Detección y Astropartículas; ArgentinaFil: Asorey, Hernán Gonzalo. Comisión Nacional de Energía Atómica. Centro Atómico Bariloche; Argentina. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Patagonia Norte; ArgentinaFil: Sidelnik, Iván Pedro. Comisión Nacional de Energía Atómica. Gerencia del Área de Energía Nuclear. Gerencia de Ingeniería Nuclear (CAB). División Neutrones y Reactores; Argentina. Consejo Nacional de Investigaciones Científicas y Técnicas. Centro Científico Tecnológico Conicet - Patagonia Norte; ArgentinaFil: Castromonte, C.. Universidad Nacional de Ingenieria, Lima; PerúFil: Fauth, A.. Universidade Estadual de Campinas; Brasi
Adición de ceniza de la paja de trigo al 5%, 10%, 15% y su influencia en la resistencia a la tracción indirecta del concreto patrón f´c=210 kg/cm2, Huaraz 2018
El objetivo principal de este trabajo de investigación es determinar la influencia de la adición de ceniza de paja de trigo a la resistencia a la tracción indirecta f'c = 210 kg / cm². Para ello se utilizó un método. Después de la investigación, el diseño de la investigación es experimental, según ASTM C. El estándar 31M, el número total de muestras y la muestra es de 36 briquetas, el diámetro es de 6 \\\\\"de diámetro y 12\\\\\" de alto, se observó el desempeño del núcleo de concreto. 7 días, 14 días y 28 días, y curado a la temperatura del agua y al ambiente normal de la zona. La prueba de hipótesis utilizará SPSSV 26. Se puede encontrar que la adición de ceniza de paja de trigo en una proporción de 5%, 10% y 15% puede aumentar la resistencia a la tracción indirecta, confirmando así la influencia de la ceniza de paja de trigo en la ceniza de la planta. La resistencia a la tracción indirecta del concreto f´c = 210 kg / cm2 con diferentes proporciones de ceniza añadida a la mezcla experimental de hormigón, que se diseña según el método ACI para hormigón con F´c = 210 kg / cm2.Tesi
Producción de biocombustible a partir de residuos de flora bentónica del distrito de Marcona, 2018
La presente investigación se realiza con el objetivo de producir adecuadamente
biocombustible a partir de los residuos de flora bentónica del distrito de Marcona, 2018; con
el propósito de definir las condiciones operativas para su desarrollo y determinar la calidad
del biocombustible obtenido. Esta investigación tiene un diseño experimental, preexperimental; de tipo aplicada a nivel explicativo. Comprende un desarrollo continuo de
diferentes etapas que inicia desde el recojo de algas marinas de especie Macrocystis pyrifera,
la recopilación de información, elaboración de gráficas y análisis de resultados que permiten
integrar las variables. Se realiza tres tratamientos iniciales con tres repeticiones en cada una,
con muestras de 30g cada una, reportándose extracciones de aceite con mejores resultados
para la deshidratación al sol, considerando este tratamiento para el desarrollo experimental
en macro y llevando a la fase de transesterificación se agregó metóxido de sodio, esto
produjo la separación de las fases, lo que conllevo a la obtención del biocombustible siendo
equitativo al ingreso de aceite. El producto paso por análisis para la determinación de la
calidad y poder calorífico, según los resultados obtenidos para las propiedades evaluadas del
biocombustible como densidad de 0,8999g/mL, viscosidad cinemática a 40°C de 2,3314 cSt,
número de acidez de 0,344mg KOH/g, residuo de carbón de 0,024% m/m y cenizas
sulfatadas de 0,017% m/m; en cuanto al poder calorífico de 38 MJ/kg a 40 MJ/kg.
Llegándose a la conclusión que las propiedades para determinar la calidad de biocombustible
a partir de muestras de Macrocystis pyrifera cumplen con las siguientes normas y
especificaciones: EN 14214, ASTM D6751, ANP N°7/08 y NTP 321.125.2008; sin embargo
la viscosidad cinemática a 40°C cumple solo con las dos primeras normas mencionadas; y
en cuanto al poder calorífico medido, llega a cumplir con el rango de 38MJ/kg a 40MJ/kg
establecido para los éster metílicos
Aprovechamiento de residuos lignocelulósicos del Saccharum officinarum por pirólisis para la obtención de bio-oil, Chongoyape 2018
En esta investigación se tuvo como objetivo general evaluar la eficiencia del
aprovechamiento de residuos lignocelulósicos del Sacharum Officinarum en la obtención de
bio-oil, Chongoyape; en el cual se recolecto 15 kg de hojas de caña de azúcar en verde para
luego ser secado por dos días al aire libre con el fin de reducir la cantidad de agua. Para
obtener el bio-oil se utilizó la pirólisis con reactor al vacío, los tratamientos empleados
fueron tres temperaturas 400ºC, 550ºC y 650ºC; se utilizó una muestra de 50 g con tamaño
de partícula de 0.85 mm para entrar al reactor. Se trabajó con una velocidad de calentamiento
promedio de 9.06°C/min, la presión de la pirólisis se mantuvo en 16.66 kPa, la temperatura
del horno 1100ºC, la temperatura del baño de enfriamiento se mantuvo controlada a menos
1 ºC. Los resultados en gramos de los productos obtenidos se determinaron por diferencia,
para el líquido y sólido, por diferencia de pesos de tren de condensación y del reactor al
inicio y final. La aplicación de los tratamientos tuvo una duración de 12 días. Los resultados
obtenidos fueron para el tratamiento Nº1 (400ºC) 41.5%, en el tratamiento Nº2 (550ºC)
42.5% y el tratamiento Nº3 (650ºC) 39.4%. Siendo la temperatura óptima que maximizó el
rendimiento la de 550ºC
Disminución de arsénico por el método de oxidación solar del agua subterránea del distrito San Juan Bautista, Iquitos 2018
Este estudio presenta como objetivo disminuir el arsénico presente en el agua
subterránea del distrito de San Juan Bautista - Iquitos, por el método de Oxidación
Solar. La población para esta investigación fue un depósito de agua que extrae agua de
la capa freática, por ello de acuerdo con el Protocolo Nacional de Monitoreo de Calidad
del Recurso Hídrico Superficial (Resolución Jefatural N° 010-2016-ANA), se admitió
una muestra de 10 litros, la cual fue no probabilística ya que se empleó un muestreo
conveniente. Medir los parámetros fisicoquímicos: conductividad (µS/cm), turbidez
(NTU), temperatura (°C) y pH de la muestra tomada, seguidamente se separó un litro de
agua para evaluar las concentraciones iniciales de arsénico obteniendo como resultado
0.0385 mg/L. A los 09 litros de muestras restante se separó de litro en litro en 09
botellas PET distintas, cada una usando tres diferentes dosis de alambre de hierro N° 16
(0.5 gr, 1 gr, 2 gr) contiene 98% de hierro y jugo de limón de otras tres variedades de
Citrus Aurantifolia Swingle en diferentes dosis (01, 02, 03 gotas) se expusieron a la
radiación solar inclinada 20° al norte con ácido cítrico al 6,85% en diferentes tiempos
(02, 04 y 06 horas), tuvieron una reducción del 85% en arsénico. Los resultados indican
que los métodos de oxidación solar reducen de manera eficaz el grado de arsénico y a su
vez es sencillo de aplicar en otros lugares con la misma realidad problemática
Análisis metalúrgico mediante cinética de flotación y diseño experimental para la obtención de un concentrado de plata (Ag) a partir de un mineral polimetálico Pb-Ag-Zn-Au, contaminado por cemento
La presente tesis tiene por objetivo el análisis metalúrgico mediante el uso, principalmente, de dos métodos: cinética de flotación y diseño experimental para la obtención final de un concentrado de plata, a partir de un mineral polimetálico Pb- Ag-Zn-Au, contaminado por cemento. El tipo de la investigación que se siguió fue la combinación de exploratoria, descriptiva y explicativa. La metodología seguida, utiliza los planes de trabajo, técnicas de experimentación y diálogos en reuniones. La investigación nos brindó las siguientes principales respuestas: a un pH: 9-10, recuperación en el concentrado final de plomo: 89%Ag, 82.05%Au, 91.90%Pb, 56.24%Zn, 48.28%Fe, asimismo, el mineral puede flotar a pH elevado, pero tanto el grado como la recuperación se ven notablemente perjudicados, los reactivos utilizados en planta, para la depresión de pirita, son antagónicos. Ante ello, las principales conclusiones son: (a) la flotación del mineral principal, flotación de plomo (con contenido de Au y Ag), no es recomendable a un pH mayor a 10.5, mientras que se justifica el proceso en el rango pH de [8 a 10.5] con un esquema recomendado en las conclusiones de esta tesis.(b) Debido al desarrollo de las distintas pruebas (con pH:[9-11]) se recomienda trabajar con un tamaño de partícula de 130 pm en el mineral, (c) la utilización del esquema recomendado de reactivos es beneficiosa para la concentración porque mejora el rendimiento en la flotación de plomo y desplaza, en buena medida, la concentración de Au y Ag del área de flotación de Zn al de Pb. Finalmente, la fortaleza del esquema logrado se sitúa en: terminar definitivamente con el uso de compuestos de Cianuro de Zinc (Zn(CN)2) en el proceso, así como la considerable reducción de la inversión en reactivos como: Metabisulfito de Sodio (Na2SsO2), Sulfato de Zinc (ZnSÜ4) y el retiro de Xantato Amilico de Potasio PAX (Z-6) y mezclas injustificadas como PAX/SIPX, siendo remplazado este último por Xantato Isopropílico de Sodio SIPX (Z-11).The objective of the present thesis is metallurgical analysis through the use of two methods mainly: flotation kinetics and experimental design for the final obtaining of a silver concentrate, from a polymetallic mineral Pb-Ag-Zn-Au, contaminated by cement. The type of research that followed was the combination of exploratory, descriptive and explanatory. The methodology followed uses the work plans, experimentation techniques and dialogues in meetings. The research gave us the following main answers: at a pH: 9-10, recovery in the final lead concentrate: 89% Ag, 82.05% Au, 91.90% Pb, 56.24% Zn, 48.28% Fe, also the mineral can float at high pH but both the degree and recovery are significantly impaired, the reagents used in plant, for pyrite depression, are antagonistic. Given this, the main conclusions are: (a) the flotation of the main ore, lead flotation (with Au and Ag contents), is not recommended at a pH greater than 10.5, while the process is justified in the pH range of [8 to 10.5] with a scheme recommended in the conclusions of this thesis. (b) Due to the development of the different tests (with pH: [9-11]) it is recommended to work with a particle size of 130 pm in the mineral, (c) the use of the recommended reagent scheme is beneficial for the concentration because it improves the yield in the flotation of lead and displaces, to a large extent, the concentration of Au and Ag from the flotation area of Zn to that of Pb. Finally, the strength of the achieved scheme is placed in: definitively ending the use of Zinc Cyanide compounds (Zn (CN)2) in the process, as well as the considerable reduction of the investment in reagents such as: Sodium Metabisulfite (Na2S5O2), Zinc Sulphate (ZnSO4) and the remove of Amyl Potassium Xanthate PAX (Z-11) and unjustified mixtures such as PAX/SIPX, the latter being replaced by Sodium Isopropyl Xanthate SIPX (Z-11).Tesi
Tratamiento de los residuos del proceso Jarosita de la industria metalúrgica del zinc, con la finalidad de mitigar este pasivo ambiental
El proceso de lixiviación del zinc (Zn) genera cantidades importantes de residuos sólidos en forma de jarosita, producida para eliminar hierro (Fe) y sulfato de las soluciones de Zn, las cuales se almacenan en presas de residuos. En la presente tesis se hace un estudio de las jarositas provenientes de una planta de refinación en México, que tiene por objetivo mitigar este pasivo ambiental; para lo cual esta jarosita fue caracterizada por diversas técnicas y se reporto contenidos de plata (Ag) de 357 g/t, oro (Au) de 0.76 g/t, y un tamaño de partícula D80 de 19 µm; con las primeras pruebas de cianuración se confirmo su naturaleza refractaria y estabilidad, por lo tanto se evaluaron procesos de descomposición alcalina a temperaturas entre 30 a 90˚C, para liberar la Ag y obtener recuperaciones de 99.9% de Ag a las 6 horas de iniciado el proceso. Además del cianuro se evaluó el uso de tiosulfato y tiourea como agentes lixiviantes para la Ag. El tiosulfato de sodio se presenta como la mejor opción con una recuperación de 99.4% a las 2.5 horas de iniciado el proceso considerando el tiempo de descomposición, y la baja toxicidad del reactivo.
Además se caracterizaron y evaluaron la movilidad de elementos de los residuos generados encontrándose que el proceso de descomposición alcalina-lixiviación en simultáneo se encuentran dentro de las normas ambientales existentes; para el proceso de descomposición térmica y lixiviación con tiosulfato se hallaron altos niveles de Cu, Zn, Fe y Pb que hacen suponer que requieren un mayor tiempo de lavado antes de su disposición, en su composición se reportó hematita y magnetita que podrían ser utilizados en nuevas aplicaciones.The process of leaching of zinc (Zn) generates significant amounts of solid waste in the form of jarosite, produced for removing iron (Fe) and sulfate of the solutions of Zn, which are stored in waste dams. This thesis is a study of jarosites from a refinery plant in Mexico, which aims to mitigate this environmental liability, for which the jarosite was characterized by various techniques and reported content of silver (Ag) of 357 g / t gold (Au) of 0.76 g / t, and a D80 particle size of 19 microns, with the first tests cyanidation was confirmed its refractory nature and stability were evaluated therefore alkaline decomposition processes at temperatures between 30 to 90 ˚ C, to release the Ag and obtain recoveries of 99.9% Ag at 6 hours into the process. Addition of cyanide was evaluated using thiosulfate and thiourea as leaching agents for Ag Sodium thiosulfate is presented as the best option with a recovery of 99.4% at 2.5 hours into the process considering the time of decomposition, and low toxicity of the reagent.
Were characterized and also evaluated the mobility of elements of the waste generated was found that the decomposition process alkaline-simultaneous leaching are within existing environmental standards, for the thermal decomposition process and leaching with thiosulfate were found high levels of Cu, Zn, Fe and Pb which suggest that a longer require washing prior to disposal, its composition was reported hematite and magnetite that could be used in new applications.Tesi
Medida de la tendencia de la temperatura en la costa mediterránea
El cambio climático ha sido objeto de una intensa investigación en los últimos años. Una variable que mide directamente este cambio es la temperatura. Por lo tanto, este estudio analiza las principales características y la tendencia de la temperatura registrada en la costa mediterránea. Se investigó un intervalo de medición para seleccionar estaciones con el mismo periodo de medición. Para ello, se consideraron las temperaturas máximas y mínimas registradas durante 40 años en 52 estaciones. Finalmente, se calcularon ciertos estadísticos para clasificar las estaciones según sus valores, formando tres grupos con un contraste de alrededor de 5 °C. Los valores mas bajos se alcanzaron en el Mar Negro, mientras que los más altos se obtuvieron en latitudes bajas. La asimetría fue ligeramente positiva en la mayoría de las estaciones. Además, las distribuciones de temperatura eran más planas que la distribución gaussiana. La última parte de este estudio considera la tendencia de la temperatura. Esto fue alrededor de 0.02 °C por año para la temperatura máxima y ligeramente mayor para la temperatura mínima. Además, el ciclo anual presentó la mayor amplitud en el Mar Negro y la más baja en estaciones con una latitud menor. Finalmente, la tendencia de la amplitud anual fue de 0.02 °C por año, similar al valor de la tendencia anual.Grado en Físic
Estudio de polarización del barión Λ producido en interacciones fotón-nucleón
Usando datos provenientes del experimento FOCUS/E831 se realizó un estudio de la polarización de los bariones Λ (y su respectiva antipartícula) producidos a través de la interacción de un haz de fotones (de energía media = 180 GeV/c) con un blanco segmentado de óxido de berilio. Se usó una muestra conteniendo alrededor de 1480 eventos de la partícula Λ que decayeron a través del canal Λπ para estudiar la distribución angular de la partícula Λ en el sistema referencial de reposo de la partícula Λ. Esto permitió obtener el producto “αP”, donde “α” es el parámetro de asimetría del decaimiento débil, y P es la polarización de Λ. También se realizó un estudio de la dependencia de “αP” con el momento transversal (p_T). Los resultados preliminares muestran que las partículas Λ son producidas no polarizadas, indicando que, diferente de lo que sucede en la hadroproduccion, los efectos del spin no son importantes en la fotoproducción.Brasil. Ministério da Educação. Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (Capes)Brasil. Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq
Recommended from our members
Study of correlations between photoproduced pairs of charmed particles at Experiment E831/FOCUS
The authors present the study of the charm-pair correlations produced in photon-nucleon interactions at <E{sub {gamma}}> = 175 GeV/c, by the Fermilab fixed target experiment E831/FOCUS. The E831/FOCUS experiment produced and reconstructed over one million charm particles. This high statistics allows the reconstruction of more than 7000 charm-pair mesons D{bar D}, 10 times the statistic of former experiments, and also allows to get, for the first time, about 600 totally reconstructed charm-pairs in the DD{sub s} and D{Lambda}{sub c} channels. They were able to study, with some detail, the kinematical correlations between the charm and anticharm particle forming a pair, in the square transverse momentum (p{sub T}{sup 2}), azimuthal angle difference ({Delta}{phi}), rapidity difference ({Delta}y) and the charm-pair mass variables. They observe some correlation for the longitudinal momenta, and a significant correlation for the transverse momenta of the charm and anticharm particles. They compare the experimental distributions with theoretical predictions based on the photon-gluon fusion model (PGF), for the production of c{bar c} quarks, and the standard Lund hadronization model. These models are implemented by the PYTHIA Monte Carlo event generator. The PYTHIA program allows the inclusion, in the simulation, of non-perturbative effects that have been shown to be important for charm production. In order to compare data and simulation, they have generated two Monte Carlo samples, the first one set to favor the production of D{bar D} pairs (MCDD2), and the second one set to favor the production of DD{sub s} and D{Lambda}{sub c} pairs, where each one uses different functions and parameters values for the theoretical models in the simulation. They observe, for the correlation distributions, that the set of parameters used by the MCDD2 model together with the intrinsic transverse momentum (k{sub {perpendicular}}) of the partons inside the nucleons, has a better agreement with data distributions than the one used by the MCDSLC model. Finally, the relative pair/anti-pair yield production ratio is calculated for five sets of charm-pairs, D{sup +}D{sup 0}, D{sup +}D{sub s}{sup -}, D{sup 0}D{sub s}{sup -}, D{sup +}{Lambda}{sub c}{sup -} e D{sup 0}{Lambda}{sub c}{sup -}, both for data as well as for the two Monte Carlo samples. They observe that the MCDSLC model predicts charm-pair yield production ratios closer to the yield ratios data than the MCDD2 model
- …