1,721,057 research outputs found

    He-irradiation effects on glass-ceramics for joining of SiC-based materials

    No full text
    CaO-Al2O3 (CA) and SiO2-Al2O3-Y2O3 (SAY) glass-ceramics are promising candidates for SiC/SiC indirect joints. In view of their use in locations where high radiation level is expected (i.e. fusion plants) it is important to investigate how radiation-induced damage can modify the material microstructure. To this aim, pellets of both types were irradiated with 5.5 MeV 4He+ ions at an average temperature of 75 °C up to a fluence of almost 2.3x10^18 cm^ -2. This produces a displacement defect density that increases with depth and reaches a value of about 40 displacements per atom in the ion implantation region, where the He-gas reaches a concentration of several thousands of atomic parts per million. X-ray diffractometry and scanning electron microscopy showed no change in the microstructure and in the morphology of the pellet surface. Moreover, a transmission electron microscopy investigation on cross-section lamellas revealed the occurrence of structural defects and agglomerates of He-bubbles in the implantation region for the CA sample and a more homogeneous He-bubble distribution in the SAY pellet, even outside the implantation layer. In addition, no amorphization was found in both samples, even in correspondence to the He implantation zone. The radiation damage induced only occasional micro-cracks, mainly located at grain boundaries (CA) or within the grains (SAY

    Bioactive Titanium Surfaces Enriched with Silver Nanoparticles Through an In Situ Reduction: Looking for a Balance Between Cytocompatibility and Antibacterial Activity

    Get PDF
    This research aims toward an antibacterial and osteoconductive Ti6Al4V surface by chemical etching–oxidation treatment and in situ reduction of silver nanoparticles. Starting from a previously developed process, already proved to enhance the osteoinductive ability of titanium, different parameters are changed to tailor the amount of silver and its distribution across the surface oxide layer thickness. The samples are characterized by scanning and transmission electron microscopy, energy-dispersive X-ray spectroscopy, release of silver, biofilm formation (Staphylococcus aureus), and cytocompatibility toward human osteoblasts progenitor cells. The total amount of silver in the surface oxide layer depends only on the concentration of the silver precursor. The time of the addition of the silver precursor, during the oxidation treatment, affects the oxide layer thickness, dimension, and distribution of the nanoparticles across the surface oxide: they are larger and accumulate on the outermost layer, if the addition occurs early. The maximum ion release occurs after 24 h and lasts up to 14 days; the later addition of silver precursors leads to sustaining the silver release for a longer time. The samples prepared with the higher concentration of the silver precursor are bactericide, but highly cytotoxic, whereas the other ones are bacteriostatic and moderately cytotoxic
    corecore