1,720,969 research outputs found

    Application of Nanocomposit Of Al2O3/Activated Carbon Prepared by Hydrothermal Process for Phenol Removal

    Full text link
    Nancomposite of Al2O3/activated carbon was prepared from the mixture of alumina oxide (Al2O3) and activated carbon from palm oil shell under the mixture of aquabidest and ethanol (1:1). The mixture was treated by hydrothermal process at 250 oC for 3 h. Resulted Al2O3/ activated carbon was characterized using SEM/EDX for studying the morphology structure of activated carbon and composite showing a like flower structure attached on the surface. The chemical compositions were 73.18%, oxygen 23.72%, aluminium 2.30%, dan silica 2.00%. The efficiency  of composite was investigated for removal of phenol in aqueous solution. The maximum adsorption of phenol was obtained at pH 2, adsorbent weight 2 g, contact time 60 min and phenol concentration 100 ppm

    Konversi Sitral Dalam Minyak Atsiri Kemangi (Ocimum citriodorum) Dengan Metode MAOS (Miuowave Assisted Organic Synthesis)

    No full text
    Konversi sitral dari daun kemangi dengan katalis basa heterogen KF/Al2O3 menggunakan metode MAOS telah dilakukan. Metode ini merupakan metode pengembangan yang ramah lingkungan. Penelitian akan mempelajari pengaruh rasio KF/Al2O3 terhadap sifat basa katalis dan juga merupakan pengaruh perkembangan terhadap produk konversi sitral dari kemangi.Hasil penelitian menunjukkan bahwa rasio terbaik untuk katalis KF/AI2O3 yaitu 30% untuk pelarut Gliserol dan 40% Etilen glikol, ditunjukkan dengan adanya OH pada pita serapan 3450 cm-1 dan menunjukkan AlF63- strecthing dari K3AlF6 pada pita serapan 586 cm-1 yang tajam. Hasil produk konversi sitral kemangi dengan pelarut Gliserol menghasilkan 6-methyl-5-hepten-2-one, 1,4-hexadiena, 3,3,5-trimethyl dan cis-verbenol sedangkan penggunaan pelarut Etilen glikol menghasilkan feniculin/l-(3-methyl-2-butenoxy_-4-(1propenyl) benzene yang sama hasil konversi dengan sitral standar. Persentasi produk dengan pelarut Gliserol 6.8%, 1.80%  dan 2.22% dan pelarut Etilen gikol sebesar 6.65%

    Karakterisasi Dan Modifikasi Karbon Aktif Tempurung Kelapa Sawit Dengan Asam Nitrat Untuk Menjerap Logam Besi Dan Tembaga Dalam Minyak Nilam

    No full text
    Modification of activated carbon has been conducted using nitric acid (HNO3). Characterization unmodified and modified activated carbon follow type I of nitrogen adsorption isotherm showed microporous material. Langmuir surface area of 253,6 m2/g to 491,6 m2/g. Identification of fungtional groups by fourier transform infrared spectrometer and Boehm titration. An increasing oxygen group on phenol of 0,0399 meq/g to 0,1987 meq/g showed acid character. Unmodified and modified activated carbon by nitric acid used as an adsorbent. The activated carbon to adsorp metal applied Fe and Cu in Patchouli oil. The metal testing by flame - atomic absorption spectrophotometer. Maximum capacity of Fe sorption in unmodified activated carbon is 9,01 ppm/g and modified activated carbon is 12,16 ppm/g Maximum capacity of Cu sorption in unmodified activated carbon is 2,25 ppm/g and modified activated carbon is 2,85 ppm/g

    Perubahan Komponen Utama Pada Minyak Atsiri Selasih Ungu (Ocimum Conum, Sims) Dengan Metode Microwave Assisted Organic Synthesis (MAOS) Menggunakan Katalis KF/Al2O3

    No full text
    Penerapan metode MAOS (Microwave Assisted Organic Synthesis) pada minyak atsiri selasih ungu (Ocimum Canum, Sims) telah dilakukan. Dalam penelitian ini KF/AI2O3 digunakan sebagai katalis, gliserol dan etilen glikol sebagai pelarut. Katalis dikarakterisasi dengan FTIR dan hasil menunjukkan penampakan tiga spektra: K3AIF6, KOH dan K2CO3. Hasil optimasi waktu dan konsentrasi yang diperoleh yaitu 6 menit pada KF/Al2O3 10% untuk pelarut gliserol dan 2 menit pada KF/Al2O3 20% untuk pelarut etilen glikol